Galvanic Corrosion Protection with the EZA Technology

Galvanic Corrosion Protection with the Embedded Zinc Anode (EZ-Anode) since 13 years

The first installation with the EZ-Anode was realized in 2007 at the Alplgraben Bridge in Styria (A) as a R&D project with a projected service time of minimum 7 years - now, after 13 years the system is still fully operable. Since then projects have been realized in Austria, Netherlands, Switzerland, Dubai, Abu Dhabi, Florida (USA), Germany. Representative projects are listed below.

icon 14 Years Of EZ-Anode

icon ICCRRR 2018 Galvanic Corrosion Protection - Field Experience

EZA Installation at an Alpine Tunnel Entrance in Obdach (Styria, A), national road B78

The SEZAC (shrinkage controlled embedded zinc anode cement) galvanic protection system was chosen for evaluation of a maintenance free corrosion protection system that allows reliable corrosion protection without extensive concrete repair works. The SEZAC system was applied in July/August 2018 on an area of 20 m2 (figure 10). The SEZAC galvanic anode was covered with an epoxy coating from SIKA certified for tunnel applications- Sikagard-332 TU, topped with Sikagard-260 WPU as a UV protective coating.

 

 

Seaside appartment buildings in Dordrecht (NL) with the embedded zinc anode (EZA), 2015

installed by Vogel Kathodische Bescherming B.V., accompanied by CPS (www.cp-supplies.nl) representing EZA technology exclusively in the BENELUX 


 

Seaside appartment buildings in Egmond an Zee (NL) with the embedded zinc anode (EZA), 2014

 


Parking Deck Saas Fee

The EZA System was applied July 2011 for demonstration purposes for the corrosion protection of the pre-stressed steel reinforcement of the central parking deck in Saas-Fee (CH)

 

Alplgraben Bridge

The EZA System was integrated within the general refurbishment of the Alplgraben bridge in Styria (A) as a technical solution to stop reliably corrosion of the steel reinforcement of the abutment.

icon·Project Report GCP Alplgraben Bridge

 


 

New References

25 years Composite Microcapillary Matrix

Read more »
 

Galvanic Corrosion Protection with the EZA Technology

Read more »
 

Application of CASTQ Composite Quantum Anode

Read more »
 

MO-DAC at IBAC of RWTH Aachen

Read more »

Recent Posts

CORTEM 2026

Read more »
 

CARRS 2025

Read more »
 

Concrete Solutions 2025

Read more »
 

ICCRRR 2024

Read more »
 

ICCRRR 2022

Read more »